The spall is reduced by line x not stopped. You would need to run soft armor in front to catch the spall.
The spall is reduced by line x not stopped. You would need to run soft armor in front to catch the spall.
There are numerous you tube videos on spalling. The ar500 plates with the build up not just the single coating are showing 99% containment.
Don't be stupid!!!!!
The Great Kazoo's Feedback
"when you're happy you enjoy the melody but, when you're broken you understand the lyrics".
Not as much as from out the back. Spalling is the Kinetic Energy (KE) from the projectile transferring to the plate and a portion(s) of the plate breaking off and continuing as a new projectile(s). The KE is transferred in the original direction unless acted upon by an outside force (Newtons 1st Law). Thus, spalling is most commonly seen with parts of the steel broken off the back of the plate where the heat and energy of the round has weakened the integrity of the steel. This is why ceramic is used as it dissipates heat better than steel and a woven ceramic/kevlar firbrous blend (ESAPIs) has better multiple impact protection than sold steel.
The Great Kazoo's Feedback
"when you're happy you enjoy the melody but, when you're broken you understand the lyrics".
"There are no finger prints under water."