    Casting, not a forging, and using the wrong alloy for the job (beverage cans are 3004 or 3104), so it's good he made it beefier than a standard lower profile. Looks like he didn't end up with any obvious voids, so it should do just fine.

    Very neat to watch, though!
    "The only real difference between the men and the boys, is the number and size, and cost of their toys."
    NRA Life, GOA Life, SAF Life, CSSA Life, NRA Certified Instructor Circuits' Feedback

  2. #2
    Gong Shooter meatman's Avatar
    Join Date
    Apr 2010
    Location
    NW Arvada
    Posts
    400

    Default

    Quote Originally Posted by Circuits View Post
    Casting, not a forging, and using the wrong alloy for the job (beverage cans are 3004 or 3104), so it's good he made it beefier than a standard lower profile. Looks like he didn't end up with any obvious voids, so it should do just fine.

    Very neat to watch, though!
    Oops. Not up on my metallurgic processes. Cast, sorry, not forged.